Etching tantalum


[ Follow Ups ] [ Post Followup ] [ Return to Ask the Experts Metallography Forum ] [ FAQ ]

Posted by Philip on December 29, 2009 at 10:21:57:

I currently have a mixture of HF/HNO3/H2O at 1:1:2 by volume respectively. It contains a maximum of 30% HF. Do you think I can work with this to etch tantalum samples?

What do you recommend?